Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vZmVD-0000TUC; Mon, 16 Dec 96 17:31 CST |
Content-Type: |
TEXT/PLAIN; CHARSET=US-ASCII |
Old-Return-Path: |
|
Date: |
Mon, 16 Dec 1996 15:12:17 -0800 |
Precedence: |
list |
Reply-To: |
|
cc: |
|
MIME-Version: |
1.0 |
Status: |
O |
Priority: |
Normal |
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
X-Loop: |
|
X-Mailing-List: |
|
Resent-Message-ID: |
<"odiNM3.0.WjS.5lTjo"@ipc> |
Subject: |
|
From: |
|
Resent-From: |
|
From [log in to unmask] Tue Dec 17 15: |
11:15 1996 |
Resent-Sender: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
From: Michael Barmuta <[log in to unmask]>
Date: Mon, 16 Dec 1996 14:56:47 pst
Subject: Re: diazo problems during lpi imaging
To: RICK TAORMINO <[log in to unmask]>
Cc: [log in to unmask]
Rick:Your LPI mask is under tack cured,there's still solvent in it.
Try raising your oven temp up to 200-208F.You may want to try
approaching this in 5F jumps.You probably also need to reduce your
dwell time in the oven by 25-35%(the higher the tack temp the less
time in the oven).I'm assuming you are using a conveyerized tunnel
oven and the 68 minutes is the time "in the box".One word of caution
it's a fine line balancing act between fully tacking the mask to hold
webs and eliminate mask on the phototools vs. locking the mask in on
pads and holes.Don't go too far.You should also bring in your
friendly Dexter Hysol rep to help.Good Luck!
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett Wa.
(206)356-6076
On Mon, 16 Dec 1996 10:00:04 -0800 RICK TAORMINO wrote:
> From: RICK TAORMINO <[log in to unmask]>
> Date: Mon, 16 Dec 1996 10:00:04 -0800
> Subject: diazo problems during lpi imaging
> To: [log in to unmask]
>
> I am having 2 problems with our diazo artworks during lpi imaging.
>
> After as few as 10 exposures, the film starts to develop a white haze (a
> "ghost" circuit image) on the emulsion side. If caught soon enough, it can
> be fairly easily wiped off.
>
> The other (more serious) problem is uncured ink from the board's holes
> depositing on the artwork. I either need a way to prevent this, or an easy
> way of removing it from the film (film cleaner works marginally ok).
>
> Here are the facts: We use Duratool film from Rexham Graphics. We have a
> Technilith ammonia developer from James River running at 155 degrees. Our
> uv density readings are around 4.6. Our lpi is Dexter Hysol SR8100R
> (SR8300). We tack cure the lpi at 188 degrees for 68 minutes.
>
> I'm sure you need more facts (nobody ever gives enough), so lay 'em on me!
>
> Thanks in advance,
> Rick
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To unsubscribe from this list at any time, send a message to: *
> * [log in to unmask] with <subject: unsubscribe> and no text. *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
> ***************************************************************************
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|