Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vYCyZ-0000bsC; Thu, 12 Dec 96 09:23 CST |
Content-Type: |
TEXT/PLAIN; charset=US-ASCII |
Old-Return-Path: |
|
Date: |
Thu, 12 Dec 1996 22:18:41 +0800 (HKT) |
Precedence: |
list |
Resent-From: |
|
Message-ID: |
|
MIME-Version: |
1.0 |
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
From [log in to unmask] Thu Dec 12 16: |
03:21 1996 |
Subject: |
|
From: |
|
X-Loop: |
|
Sender: |
|
Resent-Message-ID: |
<"Bscex3.0.ouO.QD2io"@ipc> |
Resent-Sender: |
|
Parts/Attachments: |
|
|
Hi,
I am fairly new to the PCB industry. But when I read the book about the
reflow soldering process, it takes normally 213C as the peak soldering temp
when the melting point of the solder may be, say 183C.
My understanding is that, it takes sometime to melt and acheive a
good solder joint. But how to determine 213C? Or put it this way, what
is the minimum peak temp. one should maintain? Have you come across any
literatures that talk about it ?
Any input is appreciated.
Thanks.
Y.F. Wong
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|