Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vVdLd-0000UzC; Thu, 5 Dec 96 06:56 CST |
Encoding: |
42 Text |
Old-Return-Path: |
|
Date: |
Thu, 05 Dec 96 06:57:57 cst |
Precedence: |
list |
Resent-From: |
|
Cc: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"VxJhP3.0.rMM.mPifo"@ipc> |
Subject: |
|
From [log in to unmask] Thu Dec 5 12: |
48:19 1996 |
X-Loop: |
|
Resent-Sender: |
|
From: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Hi TechNet!
For those folks interested in getting additional information about
Impedance Spectroscopy Technology contact:
Dr. Martin Seitz at: [log in to unmask]
Mike Fredrickson at: [log in to unmask]
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Re[2]: Impedance Spectroscopy
Author: [log in to unmask] at ccmgw1
Date: 12/4/96 7:48 PM
Dr. Martin Seitz at Marquette University has been doing impedance
spectroscopy on the properties of polymer thick film resistive inks
and solder paste for several years.
Nick Biunno
Zycon Corp.
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|