TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vTVS0-0000R6C; Fri, 29 Nov 96 10:06 CST
Encoding:
74 Text
Old-Return-Path:
Date:
Fri, 29 Nov 96 10:13:32 cst
Precedence:
list
Resent-From:
From [log in to unmask] Tue Dec 3 14:
39:19 1996
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/8089
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"Emz7F.0.Qc.hdmdo"@ipc>
Subject:
From:
"ddhillma" <[log in to unmask]>
X-Loop:
Cc:
Message-Id:
Parts/Attachments:
text/plain (84 lines)
     Good Morning!
     
     I'll throw a couple of ideas out that might be contributors to your 
     bonding problems:
     
     #1- If I am reading your data correctly I don't see any nickel 
     underplate between the copper and the gold. Copper can diffuse through 
     gold at a very reasonable rate and once it reaches the surface will 
     interfere with your bonding. Most wirebonding applications I am 
     familiar with use a nickel underplate to enhance the bonding 
     characteristics (although I know of specific applications where people 
     don't have a nickel underplate - these are few and far between). Your 
     "orange stain" sounds like copper. Try conducting a SEM analysis of a 
     carefully prepared microsection.
     
     #2 - Prior to the wirebonding operation, how is the surface cleaned? 
     You may have surface contamination that is causing problems - most 
     people either do ozone or plasma cleaning prior to wire bonding.
     
     One good resource to look at is "Wire Bonding In Microelectronics" , 
     ISBN 0-930815-25-4. Good Luck.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]
     


______________________________ Reply Separator _________________________________
Subject: FAB: organic contam. on wire-bond gold
Author:  [log in to unmask] at ccmgw1
Date:    11/27/96 6:18 PM


     
     HELP - What's the secret to making wire-bondable gold?
     
     Our ppm failure rate on wire bond sites is a little too high for our 
     customer.  Smallest wire-bond pad is about .014"x .050" and wire 
     mat'l is Al (generally higher failure rates on smaller pads).  The 
     highest percentage culprit has been described as an [arguably] 
     visible "orange stain" - very thin with a Carbon/Oxygen signature.  
     Board is double-sided with the following route: Drill, panel plate 
     Cu, image & plate gold (DuPont 9020), strip resist (RR3), image 
     (cover gold), cupric etch circuitry, pumice w/brushes, LPISM 
     (Probimer-65), solvent develop, bake & UV cure, legend, ET, Entek 56. 
      Gold parameters: 83-85 knoop, Ni content: 30-40ppm, As,Cu,Pb,Co, all 
     less than 3 ppm, Gold conc. is on low side: Au strike: 0.15-0.25 
     tr.oz./gal, Au Plate: 0.4-0.6 tr.oz./gal @ ~2 ASF.
     
     Questions: 
     - What are the most common contributors to wire-bond failures? 
     - Is LPISM residue one of them?
     - Are aqueous developable LPISMs generally more successful?
     - What are the, say, 3 most critical parameters to control at deep 
       gold?
     - How critical is gold surface topography (roughness)? 
     - Are ET pin dents a failure cause?
     - Can pumice operations be detrimental to the gold surface? 
     - Is low Au concentration necessarily a liability?
     
     Any input will be greatly appreciated.
     
     J.Felts
     PC World, Toronto
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2