Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset=us-ascii |
Old-Return-Path: |
|
Date: |
Tue, 26 Nov 1996 16:03:16 -0800 |
Precedence: |
list |
Resent-From: |
|
From [log in to unmask] Tue Dec 3 11: |
40:53 1996 |
Resent-Sender: |
|
Content-Transfer-Encoding: |
7bit |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
X-Loop: |
|
Resent-Message-ID: |
<"TISuc1.0.YJC.LImco"@ipc> |
Subject: |
|
From: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vSOtq-0000SOC; Tue, 26 Nov 96 08:54 CST |
X-Mailer: |
Mozilla 2.02 (Win16; I) |
Organization: |
ABB Network Partner AB |
Message-Id: |
|
Parts/Attachments: |
|
|
Hello Technetters!
We have some boards where we have to use a no-clean flux in the
THT process. Today we are haveing problem with thease boards
in the In Circuits Test where we don't have any neadle acces beacuse
of the flux resiudals after wave soldering.
Today we are using Hollis PT500 with Hollis ultra spray station and
Lonco 23F flux.
We are now looking at some new flux and I want to here if some of
you have hade the same problem and how you solved it.
Mikael Blank
ABB Network Partner AB
721 71 Vastras
Sweden
tel: +46 21 321711
fax: +46 21 146918
[log in to unmask]
http://www.abb.se/net/SENET.HTML
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|