Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vOmK0-0000UWC; Sat, 16 Nov 96 09:06 CST |
Old-Return-Path: |
|
Date: |
16 Nov 1996 09:15:09 CST |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"sEQhj2.0.dUO.dXTZo"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Mon Nov 18 10: |
41:22 1996 |
X-Loop: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
To: [log in to unmask]
*** Reply to note of 11/15/96 23:03
From: Padman Dhanakoti 32E/064 678 - 7305
****** IBM INTERNAL USE ONLY UNLESS OTHERWISE SPECIFIED *****
Subject: Long Term Storage of PCB's
Scott, One way to have the boards coated with some kind of organic
coating such as Entek cu 56(enthone) or Ronacoat(Lea Ronal) or some
coating which other supplier provide. But do not confuse this
with Entek Plus ( which is a thicker coating). Normally the
coatings willprotect the boards up to 6 months in a sealed
aluminaum bag. Padman d
Regards, Padman Dhanakoti
***************************************************************************