Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vOUYI-0000ZNC; Fri, 15 Nov 96 14:07 CST |
Content-Type: |
text/plain; charset=US-ASCII |
Old-Return-Path: |
|
Date: |
Fri, 15 Nov 1996 13:33:53 -0600 |
Precedence: |
list |
Resent-From: |
|
Message-ID: |
|
Content-Transfer-Encoding: |
7bit |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
X-Loop: |
|
Content-Description: |
cc:Mail note part |
From [log in to unmask] Fri Nov 15 17: |
57:42 1996 |
From: |
|
Mime-Version: |
1.0 |
Subject: |
|
Resent-Message-ID: |
<"FBHSh1.0.tNE.JsCZo"@ipc> |
Resent-Sender: |
|
Parts/Attachments: |
|
|
Address,
We use .020 pitch devices extensively in our designs, 12mil lands
with 8mil spacings. The conductors widths coming from these
lands are 8mils (2.1 Cu thk; .0007 foil and .0014 plating). In addition to
other varibles, I believe the 8mil cond width is robbing much needed
heat for solderability. The 8mil cond width is out of context for
such lands and FPT devices.
Q: How much influence does the conductor really have on the wetting
of the land in reflow (No heavy copper planes in the 8 layer
lay-up)?
Q: Is there a test that can be conducted to determine the amount
heat absorbed by the land.
I am in the process of convincing Hardware Design to reduce the
conductor width for the reason above, in addition to buying real
estate.
Please advise.
John Gulley
[log in to unmask]
972-578-3928
***************************************************************************