TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vNhaI-0000W3C; Wed, 13 Nov 96 09:50 CST
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
<TechNet-d-request>
Date:
Wed, 13 Nov 1996 07:59:07 -0800 (PST)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/7649
Posted-Date:
Wed, 13 Nov 1996 07:59:07 -0800 (PST)
X-Sender:
TO:
Return-Path:
<TechNet-request>
From [log in to unmask] Fri Nov 15 09:
15:17 1996
Resent-Message-ID:
<"nzheh.0.imL.DvUYo"@ipc>
Subject:
From:
X-Loop:
Mime-Version:
1.0
X-Mailer:
Windows Eudora Light Version 1.5.4 (16)
Message-Id:
Parts/Attachments:
text/plain (78 lines)
John,

It is true that the requirements have changed from J-STD-OO1A to B for
meniscus in the solder connection.  IPC-A-610B was compatible with the
J-STD-001A.  

The condition was downgraded to "should" which is a recommendation (para
1-4, 001B).  

We should also consider that there still remain some wetting requirements
for the solder connection in the B revision.  Since solder cannot adhere to
meniscus, the wetting characteristics of the connection are affected.  

The failure mechanism reflects the fact that solder cannot wet to component
meniscus material. Severe environments could cause the resulting solder
joint to fail.  Another consideration was damage to the component, which I
cannot see except in extreme cases.  

Personally, I have seen many solder connection failures resulting from this
condition during service life of products (including class 1 and 2).  The
condition becomes doubly critical when single sided boards are employed due
to minimal solder strength and intrusion of the meniscus through the PWB.  

I don't know of any test reports regarding the condition.  If they were
available, it would have been from the Mil Spec world to justify the
Military Standard content and since they traditionally required
consideration or corrective action it became a mute point through years.  

Best regards
Mel Parrish
President, MTTC Inc.

On Tue, 12 Nov 1996 10:54:00 +0000 John McGee wrote:

"Looking for clarifications, please...In J-STD-001A, Section 6.6.4.5
-'Meniscus Spacing &Trimming' it was stated
that '...Components SHALL be mounted to provide a visible clearance between
the coating meniscus (on each lead) and the solder connection', making it
mandatory for Class 3;  If  products in Classes 1 & 2 did not meet the process
control requirements, this condition was mandatory, too.  Otherwise, it was 
a Recommended condition for Class 1 or 2.
In my pre-release copy of J-STD-001B, the statement reads ' ... Components 
SHOULD be mounted...' in that way.  I see no interpretation of the word 
'should' in section 1.4  and , as well, no differentiation among the Classes.
1) Is the interpretation cleared up in the released version of -001B?
2) Has the requirement really changed since the previous revision?
In IPC-A-610B, Section 3.2.4- 'Component Installation-Vertical - Radial 
Leaded' and 4.2.3- 'Soldering-Meniscus in Solder', the 'clearance-required' 
condition is  illustrated.  It's clearly shown that meniscus in the PTH is
unacceptable 
for Class 3 assemblies.  With certain provisos, however, meniscus in the holes 
is acceptable for Classes 1 & 2.
As a Class 2 house (for now), wary of unnecessary costs- such as those
associated with spacers or special lead forming- we periodically debate the
intent of this requirement.
3)The clearance requirement is for more than just inspectability, isn't it?
4) What aspect of reliability is potentially compromised when the meniscus 
isallowed in the holes?
5) And in what ways will this breakdown manifest itself?
6) Where may I find  technical papers or test data that will help to 
illustrate this condition?"

We can be reached at:            e-mail: [log in to unmask]
Manufacturing Technology Training Center (MTTC), Inc
543 Graaf Street                     Phone 619 446-5571 
Ridgecrest CA 93555              Fax  619 446-4337
Home Page: http://www1.ridgecrest.ca.us/~mttc/mttc.htm
Bulletin Board: 619 446-4087 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2