We do have a couple Terra Universal "dessicator" cabinets that sound like what you might need. Terra Universal has
several they could offer you directly if you want a new one.
Jeff
Message# 556149
11-NOV-1996 13:15:14.12
From: [log in to unmask]
To: [log in to unmask]
Subj: Dry Box Source?
Received: from micron.com by BOGEN1 Mon, 11 NOV 96 13:14:30 MST
Received: from relay1.micron.com by micron.com (SMI-8.6/SMI-SVR4)
id NAA26361; Mon, 11 Nov 1996 13:14:22 -0700
Received: from simon.ipc.org (IPC.ORG [168.113.24.64]) by relay1.micron.com (8.7.5/8.7.3) with SMTP id MAA00808; Mon, 11 Nov 1996 12
:58:44 -0700 (MST)
Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)
id OAA25273; Mon, 11 Nov 1996 14:00:35 -0800
Resent-Date: Mon, 11 Nov 1996 14:00:35 -0800
Received: by ipc.org (Smail3.1.28.1 #2)
id m0vN1cl-0000WKC; Mon, 11 Nov 96 13:02 CST
Resent-Sender: [log in to unmask]
Old-Return-Path: <[log in to unmask]>
Date: Mon, 11 Nov 96 14:02:31 EST
From: "Allen Hertz" <[log in to unmask]>
Encoding: 22 Text
Message-Id: <[log in to unmask]>
To: [log in to unmask]
Subject: Dry Box Source?
Resent-Message-ID: <"Y9WYD1.0.2hK.wWtXo"@ipc>
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/7596
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]
Fellow technetters:
We have been trying to identify a source for a "dry box". The "Dry
Box" is a plexiglass box (or set of boxes), usually a door in the
front, optional shelving, and a flow controller operating off readings
of relative humidity. The box is used for storing moisture sensative
plastic packaged devices (BGA, QFP, etc.) to avoid moisture
absorption. The controller is plumbed to a low humidity air source
(dry air, Nitrogen, etc.). When the relative humidity readings rise
above a preset limit, the controller flows some source gas.
In searching, the closest we have come is "Blue M" which distributes a
product called a "Dry box" but is actually a dryer, more on the lines
of an oven. Blue M suggested lab equipment manufacturers.
Any potential sources would be greatly appriciated.
Thanks in advance,
Allen Hertz
Racal-Datacom, Sunrise, FL
(954) 846-5829
allen_ [log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|