TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0tnGgJ-00009BC; Thu, 15 Feb 96 21:17 CST
X-VMS-To:
Date:
Wed, 14 Feb 1996 22:37:51 -0500 (EST)
MIME-version:
1.0
Precedence:
list
Resent-From:
Resent-Sender:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/2706
TO:
Return-Path:
X-Loop:
Message-id:
Content-type:
TEXT/PLAIN; CHARSET=US-ASCII
Subject:
From:
From [log in to unmask] Fri Feb 16 08:
56:23 1996
Old-Return-Path:
Resent-Message-ID:
<"53AYb3.0.du7.MT_8n"@ipc>
Content-transfer-encoding:
7BIT
Parts/Attachments:
TEXT/PLAIN (22 lines)

Usually the copper plate rinses are too acid for this; especially
ones with a surfactant in them.  Worst I've had was in a dragout 
after catalyst.  Stuff wouldn't plate in acid copper but the metals
it took up sure did.  Probably one of the first direct plate's in
the industry :).  Lots of these things have an exterior that protects
them from oxidizers & such.  I ended up using 2% peroxide, rinse,
mechanical scrubbing, more peroxide and rinse.  Repeat monthly.
Don't forget to let Wastetreatment know about the oxidizer before
they see it or you may see an even uglier sight then the slimy stuff.


Ok, so there is a disadvantage to working in the balmy coastal climate.