Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vEjmL-0000QPC; Sat, 19 Oct 96 17:22 CDT |
Content-Type: |
text/plain; charset=US-ASCII; X-MAPIextension=".TXT" |
Old-Return-Path: |
|
Date: |
Sun, 20 Oct 96 00:09:02 PDT |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
MIME-Version: |
1.0 |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
X-Loop: |
|
Resent-Message-ID: |
<"I2GCN3.0.XQE.8ILQo"@ipc> |
Subject: |
|
Read-Receipt-To: |
|
Content-Transfer-Encoding: |
quoted-printable |
From [log in to unmask] Wed Oct 23 14: |
32:10 1996 |
From: |
|
Message-ID: |
|
Parts/Attachments: |
|
|
Subject: Fab-Re: Question about Wedge voids
Alex
If i've well understood wedge voids, nailhead and pink ring are different effects of the same process out of control:
DRILLING.
That's true?
If yes, please i need more informations when they occur.
Thanks and sorry for my english.
***************************************************************************