Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0v8TQ1-0000TUC; Wed, 2 Oct 96 10:41 CDT |
Encoding: |
54 Text |
From [log in to unmask] Wed Oct 2 13: |
27:08 1996 |
Date: |
Wed, 02 Oct 96 05:16:38 cst |
Precedence: |
list |
Resent-From: |
|
Cc: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"mj8jb2.0.nQL.GqeKo"@ipc> |
Subject: |
|
From: |
|
Old-Return-Path: |
|
X-Loop: |
|
Resent-Sender: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Hi Jan -
I might be wrong but leaving a weak organic acid residue on the
surface of your PWA may get you into trouble down the road. What is
your use environment? Will moisture condensation end up on the
assembly? What levels of voltage/current are running in the area of
the residue? I have had a bad experience with a different Interflux
product and non-cleaned residues in my use environment. We ran an SIR
test and had an eye opening experience. I suggest you get ahold of
Doug Pauls ([log in to unmask]) of Contamination Studies Labs - he may
have some useful information.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Adipic acid
Author: [log in to unmask] at ccmgw1
Date: 10/1/96 11:51 AM
Hi all TechNetters!
I'm just wondering about a no-clean flux made by InterFlux called
interflux2005M.
Sometimes we need to put some extra flux on certain kinds of components,
and if there's not enough heat it won't burn away and leave a white
powder left on the PCB. This is to my knowledge Adipic acid (spelling?).
How does this affect the components and PCB if it's in one kind of a
place where you can't brush it off?
Of course we can use a waterwash or any similar kind of washer, but we
don't wan't that extra step in the production. Many people here at
Ericsson have diffrent theorys about if the flux do harm or not.
Anybody have any experience in this matter?
Regards,
Jan Merstrand
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|