Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0v6cAu-0000Q9C; Fri, 27 Sep 96 07:37 CDT |
Encoding: |
55 TEXT |
Old-Return-Path: |
|
Date: |
Fri, 27 Sep 96 08:44:00 PDT |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
From [log in to unmask] Fri Sep 27 08: |
56:39 1996 |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"j3ZX7.0.ZNM.RgyIo"@ipc> |
Subject: |
|
From: |
|
Status: |
O |
X-Loop: |
|
X-Mailer: |
Microsoft Mail V3.0 |
Message-Id: |
|
Parts/Attachments: |
|
|
As a micro-etch (either type) becomes saturated with copper, there is a
tendency for it to redeposit copper sulfate crystals, especially when it
hits a cold rinse. These tiny copper sulfate crystals will cause dewetting
in HASL. It is common practice to follow the micro-etch rinse with a
sulfuric acid dip of 5-10% and rinse. This redissolves the copper sulfate.
Another fix is to change (persulfate) or regenerate (peroxide-sulfuric) the
micro-etch more frequently, to prevent copper buildup in the solution.
Also, maintain enough acid in the etch (see supplier) to keep the maximum
amount of copper in solution.
Patty
----------
From: TechNet-request
To: TechNet
Subject: Re: HASL Microetch
Date: Thursday, September 26, 1996 1:30PM
As a HASL service provider we see the entire gambit of solder mask
residues. We use a persulfate based etchant at a rate of 40-60
microinches. The trade off is that it is much more difficult to rinse
than peroxide/sulfuric chemistries and can cause non-wets if not
entirely removed before entering the HAL machine.
Michael Holan
Process Engineer
Radian Electronics Div.
[log in to unmask]
______________________________ Reply Separator
_________________________________
Subject: HASL Microetch
Author: [log in to unmask] at INTERNET
Date: 9/26/96 12:57 PM
Does anyone have information, opinions or preferably data regarding micro
etching with persulfate vs sulfuric acid/peroxide chemistries? We are
currently using a sulfuric acid/peroxide based microetch at the HAL line,
and
are considering alternatives. I have seen some information which suggests a
persulfate based chemistry is better at removing solder mask residues. Any
feedback would be appreciated.
Jim Kenny
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|