Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0v5gqX-0000QBC; Tue, 24 Sep 96 18:24 CDT |
Old-Return-Path: |
|
Date: |
Tue, 24 Sep 96 16:02:26 EST |
From [log in to unmask] Wed Sep 25 12: |
12:59 1996 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<DesignerCouncil-request> |
Resent-Message-ID: |
<"U4UV-3.0.euK.6t6Io"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Cc: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Hi Don:
I am not sure who wrote about the pink ring either, but in my
experience, thermals limit the spread of the pink ring rather than
limiting pink ring itself, by limiting the cross sectional area of the
oxide that is available for chemical attack. In other words, the
total area of oxide across the top of the thermal ties is much less
than the total area of oxide available, if the site of attack was a
solid oxided reference plane. In cross sections, many times the pink
ring has spread throughout an internal land, but not all the way
across the ties connecting the land to the rest of the reference
plane, I think one of the reasons is because there was not enough area
of oxide on the ties to sustain the oxide reduction reaction.
Greg Schroeder
Hadco
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Re[2]: DES: VIAS - Thermal vs. Direct
Author: [log in to unmask] at SMTPLINK-HADCO
Date: 9/24/96 6:27 PM
I'm not sure who wrote this, but I would like to hear more. How does
a direct connect via increase the incidence of pink ring? Perhaps my
understanding of what creates pink ring is in error but I would think
the geometries and chemistries at the hole wall is the same either way.
Also, what do you TechNetters say about pink ring? Is is a functional
defect or not? How many board failures have you seen attributed to pink
ring (whether thru delamination, via failure, or whatever)? Please note
the word failures - not rejections (although that might be interesting
to know as well). As we all know, sometimes requirements are based on
"that's the way we've always done it" rather than on real data.
[log in to unmask]
Don Walker
> By eliminating thermals at via locations you significantly increase
> the probability of creating pink ring. Depending on who you talk to
> will determine if pink ring is a functional defect or not. If your
> finished specification for your board manufacturer states "No pink
> ring allowed" you are setting him up for failure. If pink ring is a
> non issue with your company and this is reflected in your
> specification this is a non issue. The diameter of the center pad,
> width of the spokes and diameter of the clearance around the center
> pad are significant factors that contribute to the amount of pink ring
> present.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
****************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05 *
****************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
****************************************************************************
|
|
|