Mime-Version: |
1.0 |
Content-Type: |
text/plain;
charset=US-ASCII |
Old-Return-Path: |
|
Date: |
Wed, 18 Sep 96 1:27:19 EDT |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
From [log in to unmask] Wed Sep 18 10: |
32:18 1996 |
Resent-Message-ID: |
<"iPe0D.0.fGF.kI0Go"@ipc> |
Subject: |
|
X-Priority: |
3 (Normal) |
X-Loop: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0v3NSS-0000SLC; Wed, 18 Sep 96 09:18 CDT |
From: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Gold pads have more then one purpose. If the gold pad is a contact connector
subjected to repeated use, the electroless nickel / immersion gold process
only deposits 2-8 micro inches of gold which may not hold up to repeated use.
We have converted several customers from HASL to both E Ni/I Au and Entek.
Cost and the end use of the board should dictate the surface finish required.
[log in to unmask] Wrote:
|
| Scott
|
| I cannot answer your question about the Enteck and the
| tarnishing, but I am
| wondering why you have selective gold plating and the
| Enteck process.
|
| The electroless gold plating can be used to ensure
| solderability of SMT
| pads. We presently populate and reflow a PCB that is
| electroless gold over
| electroless nickle. The gold plate ensures the
| solderability of the nickle
| and the thickness of the gold plate is such that you do
| not have a gold
| embrittled joint.. We have been running this in
| production for well over a
| year with no solderability problems.
|
| This process was chosen because we needed a nickle pad on
| the PCB that
| contacted a nickle terminal within the housing(like
| metals) for wear
| purposes. Originally the PCB was going to be the nickle
| plate with HASL
| and the one pad would be masked off so it would stay
| nickle. The bare
| board fabrication cost was less by using the nickle plate
| and then the gold
| plate. The other process was lengthier and required
| masking of the one pad
| during the HASL step and then removal of the mask. Since
| gold is a noble
| metal, we can leave it on the contact pad with no problems
| and the gold
| ensures the solderability of the nickle.
|
| To re-ask my question--Why have a PCB with some pads gold
| plated and the
| other Enteck, thus requiring more steps in the PCB
| fabrication when you
| could have the entire PCB electroless gold plated and
| still have proper
| solderability.
| -------------
| Original Text
| From:
| C=US/A=INTERNET/DDA=ID/TechNet-request(a)ipc.ipc.org, on
| 9/18/96 7:30
| AM:
| From: Scott Westheimer
| Date: 9/17/96
|
| Sorry if my message of last night was not very clear, but
| what can you
| expect at 2:30 am.
|
| The issue is with entek coating not the gold plating. The
| panels have
| selective gold plating on some pads and the others have
| entek. The problem
| is that when the panels are first gold plated(
| electrolydicly ), then S/M
| the entek pads are fine. However, when the panels are
| first S/M and then
| gold plated the entek pads are tarnished around the edges.
| Does anyone have
| experience with this problem.
|
| Thanks,
|
| PS Before anyone makes the comment, the boards are enticed
| after all the
| processes have been completed.
|
| **********************************************************
| *****************
| * TechNet mail list is provided as a service by IPC using
| SmartList v3.05 *
| **********************************************************
| *****************
| * To unsubscribe from this list at any time, send a
| message to: *
| * [log in to unmask] with <subject: unsubscribe> and
| no text. *
| **********************************************************
| *****************
|
|
| **********************************************************
| *****************
| * TechNet mail list is provided as a service by IPC using
| SmartList v3.05 *
| **********************************************************
| *****************
| * To unsubscribe from this list at any time, send a
| message to: *
| * [log in to unmask] with <subject: unsubscribe> and
| no text. *
| **********************************************************
| *****************
|
|
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|