Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0v3MhI-0000T3C; Wed, 18 Sep 96 08:29 CDT |
Content-Type: |
text/plain; charset=US-ASCII |
From [log in to unmask] Wed Sep 18 08: |
56:32 1996 |
Old-Return-Path: |
|
Date: |
Wed, 18 Sep 1996 09:50:48 -0400 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
Content-Transfer-Encoding: |
7bit |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
Content-Description: |
cc:Mail note part |
Subject: |
|
From: |
|
X-Loop: |
|
Mime-Version: |
1.0 |
Resent-Message-ID: |
<"rZADf2.0.e1J.Ab_Fo"@ipc> |
Message-Id: |
|
Parts/Attachments: |
|
|
There are several factors beside stencil thickness that can affect the
print thickness. The distance between the stencil and the board is
important. For stencils, I use as close to zero snap off as I can
get. Your fixturing can also affect the print thickness. If you do
not get adequate support under the board, the board can bow away from
the stencil during printing and effectively increase the snap off,
resulting in a thicker print. I use drop in workholders for each
board that I am printing to minimize this effect. I also found that
if I decreased the stencil release time, I got more consistent print
thicknesses.
______________________________ Reply Separator _________________________________
Subject: Assy: Solder Paste Height
Author: [log in to unmask] at Internet
Date: 9/16/96 4:09 PM
I am trying to determine the solder paste height based on stencil
thickness. I have noticed that with a 7mil stencil I am getting
approximately 8mils of paste height using a metal squeegee blade
regardless of pressure settings. Is this typical of the screen printing
process??
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|