Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Tue, 20 Aug 1996 21:10:02 -0400 |
Precedence: |
list |
Resent-From: |
|
From [log in to unmask] Thu Aug 22 06: |
06:45 1996 |
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Resent-Message-ID: |
<"zQqaJ3.0.OSH.Iqb6o"@ipc> |
Subject: |
|
From: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0ut1U3-0000MlC; Tue, 20 Aug 96 19:49 CDT |
Resent-Sender: |
|
X-Mailer: |
Windows Eudora Light Version 1.5.2 |
Message-Id: |
|
Parts/Attachments: |
|
|
I am experienceing a fine dusting of nodgles that show up anywhere on the
circuits especially on ground plane areas. The nodgle is dome shaped, higher
than the surrounding area and very spherical in shape. Bright acid copper,
everything in spec.I have eliminated deburr, resist (as I see it on panel
plate also only with much less frequency of occurance).Not a pit from air
inpengment a dome. Suspect a fungus in the brightener ???
Wondering if anyone else has seen anything similiar
Thanks
Wm.M.
***************************************************************************