Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0urBcZ-0000MqC; Thu, 15 Aug 96 18:14 CDT |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Thu, 15 Aug 1996 19:22:08 -0400 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
From [log in to unmask] Fri Aug 16 15: |
37:28 1996 |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"1KAiD2.0.1iL.Qzw4o"@ipc> |
Subject: |
|
From: |
|
X-Status: |
|
Mime-Version: |
1.0 |
X-Loop: |
|
Message-Id: |
<v03007800ae3960b55a9f@[146.115.113.25]> |
Parts/Attachments: |
|
|
on Thu, 15 Aug 1996 18:12:57 -0400
"3.1415" <[log in to unmask]> asked:
>What was the baking temperature?
Curie temp was 120C so I baked at 130C.
[...]
>> De-aging of ceramic capacitors is a bake above their Curie point
>> temperature. I've had to bake caps anywhere from 1 to 16 hours to de-age
>> them. No vacuum is involved.
[...]
***************************************************************************