Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset=us-ascii |
Old-Return-Path: |
|
Date: |
Thu, 15 AUG 96 10:40:40 MDT |
Precedence: |
list |
Resent-From: |
|
Cc: |
|
Content-Transfer-Encoding: |
7bit |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
From [log in to unmask] Thu Aug 15 13: |
30:37 1996 |
X-Status: |
|
Resent-Message-ID: |
<"n0dEA2.0.RAL.x5r4o"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0ur5Mz-0000NxC; Thu, 15 Aug 96 11:34 CDT |
Resent-Sender: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
There are a few controlled atmosphere(aka full tunnel) systems out there that
use entrance and exit staging chambers. Check the ATMOS 2000 from Electrovert,
or the Sigma Wave 6567 from Dover/Soltec. I am sure there are a few more out
there. We do not have a contolled atmosphere system, but they apparently
reduce dross to about a few teaspoons a month!
These systems are quite expensive.
Steve Abrahamson
***************************************************************************