Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0ur2sN-0000MeC; Thu, 15 Aug 96 08:54 CDT |
Encoding: |
17 TEXT |
Old-Return-Path: |
|
Date: |
Thu, 15 Aug 96 08:54:00 CDT |
Precedence: |
list |
Resent-From: |
|
Message-ID: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
From [log in to unmask] Thu Aug 15 13: |
27:23 1996 |
Resent-Message-ID: |
<"-k_dX3.0.rTJ.9mo4o"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Cc: |
|
X-Mailer: |
Microsoft Mail V3.0 |
Resent-Sender: |
|
Parts/Attachments: |
|
|
I will see that from time to time if excess flux residue has colleted on the
wave pallets. Try cleaning them and see what happens.
[log in to unmask]
----------
From: TechNet-request
To: TechNet
Cc: George_Cooper_at_FTL04
Subject: Solder Sticking to Wave Soldering Pallets
Date: Wednesday, August 14, 1996 02:55
Has any one found solder sticking to hard coated Al wave solder pallets?
What
caused it? We have found this on our latest solder pallets and are baffled.
[log in to unmask]
***************************************************************************