Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0uqs43-0000KoC; Wed, 14 Aug 96 21:21 CDT |
Old-Return-Path: |
|
Date: |
14 Aug 96 22:28:13 EDT |
Precedence: |
list |
X-Loop: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
From [log in to unmask] Thu Aug 15 13: |
25:42 1996 |
Resent-Message-ID: |
<"jJS9H3.0.wtK.oce4o"@ipc> |
Subject: |
|
From: |
|
Message-ID: |
|
Resent-From: |
|
Parts/Attachments: |
|
|
To: MAIL@CSERVE {INTERNET:[log in to unmask]
From: MAIL@CSERVE {INTERNET:[log in to unmask]
Subject: assy: Dross elimination
Date: 14-Aug-96 18:19
Hello TechNetter!
Question for all the wave solder folks. Have any of you
found a way to totally eliminate dross from your wave solder
machines?
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
Eliminate.......No!
Drastically reduce yes!
We have two insert atmosphere(Nitrogen) wavesoldering systems. As well
as the greatly improved quality of soldering, they
produce almost no dross in comparison to conventional systems.We
NEVER experience solder defects cause by dross being circulated in the
wave, which did happen on our previous equipment even though we
maintained the pot and pump well.
Regards
has totally eliminated dross finding its way onto the solder joints
***************************************************************************