Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Wed, 14 Aug 1996 16:31:48 -0400 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
From [log in to unmask] Wed Aug 14 14: |
22:09 1996 |
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Resent-Message-ID: |
<"rXHwC.0.d3J.LdV4o"@ipc> |
Subject: |
|
From: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0uqiU2-0000NgC; Wed, 14 Aug 96 11:07 CDT |
Cc: |
|
X-Mailer: |
Windows Eudora Version 1.4.4 |
Message-Id: |
|
Parts/Attachments: |
|
|
Irv,
I saw an article some time ago on Latest. It sounded very much like
traditional THD measurement, but with the addition of DC bias. Have
I misunderstood, and if not what is the advantage of the DC bias?
David Whalley
Loughborough University
>
>FROM: I. MEMIS, DEPT GGMG/BLDG 257-4, AISLE A, ENDICOTT
>*** Resending note of 08/13/96 13:54
> ENDICOTT ELECTRONIC PACKAGING
>SUBJECT: Fault finding on test vehicles
>=========================================================================
>SUBJECT: Fault finding on test vehicles
>The most effective system that we have for detection of "near-opens" or
>"intermittents" is using LATEST Model 10. This is described in technical
>reports that have been presented at IPC and other conferences. LATEST
>is capable of finding local 3 milliohm deviations from nominal in a
>5 ohm line. After confirming the presence of the "near-open" with LATEST
>you then start to split the net thru probing with LATEST to isolate the
>bad section. Good parts of the net show low levels of LATEST output but
>the bad sections repeat the end to end LATEST net output. If anyone is
>interested in more info, please contact me at 607-755-6022.
>Irv Memis
>IBM
>Endicott,NY
***************************************************************************