TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0uqMEr-0000LBC; Tue, 13 Aug 96 11:22 CDT
Encoding:
127 TEXT
Old-Return-Path:
Date:
Tue, 13 Aug 96 12:15:00 DST
Precedence:
list
Resent-From:
From [log in to unmask] Tue Aug 13 11:
35:46 1996
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/5725
TO:
"'IPC - Technet Input'" <[log in to unmask]>
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"3rNDB1.0.MzA.GlA4o"@ipc>
Subject:
From:
"Dill, Norm J" <[log in to unmask]>
X-Loop:
X-Mailer:
Microsoft Mail V3.0
Message-ID:
Parts/Attachments:
text/plain (137 lines)

     HV breakdown is a current topic here as well.  In a basic double sided 
application that has a continuos 7KVAC with frequencies up to 30 MHz, is 
there any advantage to using the more expensive polyimide laminate in place 
of FR4?
      Is there any truth to the rumor that polyimide is more 'arc tolerant' 
because of it's higher Tg?

      Norm Dill
      [log in to unmask]

 ----------
From: TechNet-request
To: technet
Subject: Re: DES:FAB:ASSY: Breakdown
Date: Wednesday, August 07, 1996 8:46AM

Dom Bragge asked a question on high voltage design rules: 12 mil space 1500 
V

First the caveats: The voltage you quote is definitely in the "marginal" 
area.
I believe that it violate IEC guidelines.  I would be less concerned if the
voltage represented a fault condition or was applied for a short time. A
continuous application of 1500 V is very risky.

That said, let me address your question.  There are at least four possible
failure modes.  Ranked in order of risk they are the following: dust 
buildup,
surface flash-over, dielectric failure, and air breakdown.  Let me comment 
on
the risk from each of these

Dust build up is the most serious problem.  I assume the voltage is DC (if 
it
is AC there are other problems). The fields associated with a DC voltage
attract dust.  (Think of the high voltage supply in a TV set).  Over time 
the
dust will build up and span conductors.  Under high humidity conditions, 
dust
absorbs moisture and creates a leakage path that can carbonize leading to
failure.  We have seen this failure under field conditions. The only 
solution
is to this is to maximize the separation of uncoated features and to assure
there are absolutely no pinholes in the soldermask.  Pinholes are the real
risk so a double soldermask coating should be used. A conformal coating of 
the
assembled board would also be a good idea.

Surface flash-over is the second serious risk.   Any dielectric surface
provides a breakdown path for high voltage.  The breakdown follows the
surface, so a smooth surface is riskier than a rough surface (Think of the
shape of the insulators they use on high voltage transmission lines).
Unfortunately soldermask is very smooth and 1500 volts can arc across gaps
up to 30 mils wide.  This phenomena is initiated at any "triple point" where 

air, dielectric and metal meet.  The solution is to assure that the 
conductor
is totally encapsulated.  Any soldermask pinhole is a source of an arc that
will flash to the nearest uncoated land.  Therefore you must assure pinhole
free soldermask.

I have little information on the long term reliability of either FR-4 or
soldermask under high voltage conditions.  Voltage is an acceleration factor 

in dielectric failure, but my sense is that most modern materials provide
margin and 1200 volts is not a problem.  I have seen application where
standing voltages of 300 to 500 volts gave no long term problem. I would be
willing to gamble that you could get away with 1500 volts. However there is 
a
risk of long term dielectric failure, particularly if the temperature or
humidity is high.

Air breakdown should not be a problem. The Paschen curve says that the 
maximum
spark gap for 1500 volts is about 8.5 mils.  If you assure a 12 mil space 
air
gap breakdown will not be an issue.

To summarize.  The two biggest issues with 1500 V are dust buildup and 
surface
flash-over.  The solution to both problems is to absolutely exclude 
soldermask
pinholes. (The electric field easily finds even the most minute hole on a 
line
edge).  If you can exclude pinholes and guarantee a 12 mil space I think you 

may a reasonable shot at a good system life.

Good Luck


Bob Holmes
Lucent Technologies
[log in to unmask]


------------- Begin Original Message -------------

Using 1.6mm FR4 with LPISM, we need information on how to prevent
breakdown between tracks on the outside layer separated by 12thou,
when subjected to 1500V continuously.  What sort of coatings/processes
aid this?


 --
Regards,            (A4fonHPUX9.0onHP715,710)    JNA Telecommunications
Limited                                  ___  _____     16 Smith Street
Dom Bragge    (VK2YAK)        __ / / |/ / _ |    Chatswood NSW 2067
PWB Designer, (R&Ddiv)       / // /    / __ |    AUSTRALIA
Tel: (+61 2) 9935 5792       \___/_/|_/_/ |_|    email [log in to unmask]
Fax: (+61 2) 9417 3862                           http://www.jna.com.au

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2