Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0ulhEL-0000OzC; Wed, 31 Jul 96 14:46 CDT |
Old-Return-Path: |
|
Date: |
Wed, 31 Jul 1996 16:51:00 -0400 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"byPl3.0.Qm8.iWx_n"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Wed Jul 31 17: |
30:26 1996 |
X-Loop: |
|
X-Mailer: |
Worldtalk (NetConnex V4.00a)/MIME |
Message-Id: |
|
Parts/Attachments: |
|
|
----------
From: Kelly, Pat
To: Technet
Subject: Wave solder not adhering to electrotin plated fasteners
Date: Wednesday, July 31, 1996 3:52PM
Hi there!
I need some help. We manufacture steel, threaded fasteners that broach into
printed circuit boards. These fasteners are electrotin plated for excellent
solderability. These fasteners pass the ASTM B678 solderability test
easily.
One customer is using our fasteners in a typical PCB application. After
installing our fasteners, the board is put thru a wave solder process. This
customer claims - and has given me samples - of fasteners that definitely
have not held soldered adequately.
Anyone out there please help. Why would our fasteners pass the ASTM B678
solderability test but experience trouble in a "real world" application?
Has anyone experienced a similar problem with our fasteners. Let me know.
Thanks,
Pat Kelly
Applications Engineering Manager
Penn Engineering
215-766-8853-1162
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|