Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0ulOZ8-0000LUC; Tue, 30 Jul 96 18:51 CDT |
Old-Return-Path: |
|
Date: |
Tue, 30 Jul 96 19:22:44 EST |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"v3aqx3.0.MpH.d_f_n"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Wed Jul 31 17: |
24:02 1996 |
X-Loop: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Dave et al:
From a board fabrication point of view, there is a
difference in the price of the board if "X-outs" aren't
allowed for shipment to the customer. If no "X-outs" are
allowed, the entire array of boards is generally quoted as
"one piece", and this price is divided by the number up
within the array or pallet to determine the unit price. If
"X-outs" are allowed, the board is priced out as individual
parts on the panel that will fit, given the array size and
shape. The price changes depending upon the yield factor
used by the quote system. As the parts get smaller, this
difference is enhanced.
In my experience, I have seen more customers allow
"X-outs" to one degree or another than not. Certain issues
should be worked out with the board supplier, such as:
segregating boards with "X-outs" in shipment
allowing only a certain per cent of shipped arrays to
have "X-outs" (5% is quite common)
allowing only a certain amount of "X-outs" per array
(typically 25% to 40%, depending on the number up
within the array)
The easiest way for baord fabricators to indicate a
board defect within an array is to "X" out (thus the
moniker) the bad board on both sides with a black "Sharpie".
I have seen other more sophisticated methods, such as BBI's
(bad board indicators); usually a pad or fiducial that must
be drilled out if that particular part is defective. I've
also heard that this method can cause pain during assembly
solder paste operations.
Ask your board fabricator to quote a particular
palletized part using both scenarios. This will give you an
idea of what the actual savings to you would be. Then make
your decision relative to the extra work required during
assembly.
Regards,
Tom Coyle
Field Services Engineer
HADCO Corporation
***************************************************************************