Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0ukspn-0000QTC; Mon, 29 Jul 96 08:58 CDT |
Encoding: |
38 Text |
Old-Return-Path: |
|
Date: |
Mon, 29 Jul 96 08:39:31 cst |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
From [log in to unmask] Tue Jul 30 12: |
00:42 1996 |
Resent-Message-ID: |
<"scGoe3.0.E0O.nDC_n"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Cc: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Hi David:
Could you be getting a turbulent flow/disruption in the Nordson
nozzle? What about a contaminate on the PWA that is reacting with the
postcoat to form bubbles?
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Bubbles in Conformal Coating
Author: [log in to unmask] at ccmgw1
Date: 7/26/96 11:52 AM
Has anyone ever experienced a problem with bubbles in conformal
coating when using an acrylic coating (CONAP 1171) applied with a
Nordson Select Coat system? The bubbles appear instantly as the
coating is applied. The result is a non-conforming defect per
IPC-A-610 section 7.1.2. Thank you.
David Bruni
Manufacturing Engineer
MSA
Instrument Division
(412) 776-8848
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|