Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0uXBVI-0000CXC; Fri, 21 Jun 96 14:04 CDT |
Old-Return-Path: |
|
Date: |
Fri, 21 Jun 96 12:12:39 PST |
Precedence: |
list |
Resent-From: |
|
From [log in to unmask] Fri Jun 21 15: |
28:20 1996 |
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"2AnGS2.0._u7.t8lon"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
I'm sure there's someone out there with Bellcore "listening". How do
we get this paper??
______________________________ Reply Separator _________________________________
Subject: Unidentified subject!
Author: [log in to unmask] at corp
Date: 6/21/96 11:32 AM
Folks:
Sometime ago, Bellcore published a study on copper oxidation: "The Surface
Composition of Copper with Indoor Exposures Ranging from 3 to 49 Years"
Schubert and D'Egidio, Corrosion Science 1990. They found that the copper
corrosion is similar to aluminum, to first order it passivates. After about 40
years the oxide thickness is only about 0.4 mils. Although the an indoor
environment was used, it was none the less, very aggressive!
Lee Parker
Lucent Technologies
|
|
|