We are 2nd stage drilling .220" to .250" holes at NC rout and experiencing
.020" to .030" haloing/delamination. The 2nd drill is in areas of bare
laminate (no metal pad or ground plane). Does anyone have suggestions to
prevent this? Thanks for any input.
Lyle Anderson
Electrostar-Utah
[log in to unmask]
|
|
|