Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0uPClp-0000C9C; Thu, 30 May 96 13:48 CDT |
From [log in to unmask] Wed Jun 5 16: |
09:25 1996 |
Old-Return-Path: |
|
Date: |
Thu, 30 May 96 13:53:11 cst |
Precedence: |
list |
Resent-From: |
|
Cc: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"hWRY63.0.aQH.yrUhn"@ipc> |
Subject: |
|
From: |
|
Encoding: |
43 Text |
X-Loop: |
|
Resent-Sender: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Hello Bill -
The only bad experiences that I have had with Indium solders/alloys
relates to corrosion. Some of the use environments contained enough
moisture that I had solder joint corrosion. Of coarse, these issues
were an integral part of the pwa design (amount of voltage, component
layout, etc) parameters and the end use environment - a poor material
choice selection rather than problems with indium solder. Check out
Chapter 2 for references on Indium containing solders in Solder
Mechanics: A State of the Art Assessment by Frear, Jones, and Kinsman
- there may be some information that is useful to you.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: assy:gold/indum/solder
Author: [log in to unmask] at ccmgw1
Date: 5/29/96 6:46 PM
What is the compatibility of using indum7 to gold? to solder?
some of our folks here believe that _any_ tin/indum is a bad thing (like
tin/gold)
we are planing to use Indum7 to connect a solder coated lead to a gold pad (SMT)
Bill Gaines
AeroJet (for $) IHPVA (for speed & fun)
IEPS (for info) SCCA (for trophys)
[log in to unmask]
===================================================
/| _ _ _
/_||_ |_ |
/ ||_ _| |_
==================================================
|
|
|