Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0uOIfM-00008RC; Tue, 28 May 96 01:54 CDT |
Content-Type: |
text/plain; charset="US-ASCII" |
Old-Return-Path: |
|
Date: |
Tue, 28 May 96 08:24:28 +0100 |
Precedence: |
list |
Reply-To: |
|
Resent-Sender: |
|
Content-Transfer-Encoding: |
7bit |
Status: |
O |
X-Mailing-List: |
|
From [log in to unmask] Wed Jun 5 11: |
37:28 1996 |
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
X-Loop: |
|
Resent-From: |
|
Resent-Message-ID: |
<"s4aNN1.0.8O.BCggn"@ipc> |
Content-Description: |
<A:\ipc\omega2.txt> |
Subject: |
|
From: |
|
Mime-Version: |
1.0 |
Content-Id: |
<13_60_1_833286279> |
X-Mailer: |
Ultimedia Mail/2 Lite, IBM T. J. Watson Research Center |
Message-Id: |
<9605281525.AA0016@localhost> |
Parts/Attachments: |
|
|
BLUE SMURF's Question:
The main function(s) of "OMEGA wave" in wave soldering?
We use Omega Wave on our Electrovert waver to get better fillet for
through hole components and to prevent shadowing of SMD's.
Try contacting Electrovert for the paperwork.
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Ivo de Rooij Manufacturing Process Engineer SMT/THT
@ __ __ @ @ ______
_|________ _|__|_|__|_| _____|_______| ____ |___
| // | | | // | | | || // || |
====| _____ o.|====| |________|o|==========| o. _______ ||____|| _ |====
| ________ | | ________ | |___._| | |_______| | | _ |
||________|| |_|________|_| | | |_____________|______|___|
|| || || || | | || || || ||
Fokker Elmo BV (Fokker Aviation) [log in to unmask]
Electr(on)ic Systems Civil, Military, Aircraft and Space
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~.
|
|
|