TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0uMKsr-0000CMC; Wed, 22 May 96 15:51 CDT
Old-Return-Path:
Date:
22 May 1996 13:54:58 -0700
Precedence:
list
Resent-From:
From [log in to unmask] Tue Jun 4 18:
04:39 1996
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/4285
TO:
"IPC Technet" <[log in to unmask]>
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"IhdIg.0.TO7.fvten"@ipc>
Subject:
From:
"Ralph Hersey" <[log in to unmask]>
X-Loop:
X-Mailer:
Mail*Link SMTP-QM 3.0.2
Message-ID:
Parts/Attachments:
text/plain (102 lines)
Mail*Link(r) SMTP               FWD>FAB: Fwd: Printed Circuit Board Lamination
Process

Marc and Dean

There is a good use to reuse printed board base material.  Good quality stuff
is ground up and used as a filler by the molded plastics industry.  If you
want, I can check and find out some more particulars, or perhaps Chris Rhodes
(the environmental guy) at IPC headquarters might have some better info.

Ralph Hersey
e-mail:  [log in to unmask]

--------------------------------------
Date: 5/22/96 12:54 PM
From: Dean R. Cornstubble
I am not sure if any of you can address this issue, but TechNet seemed
to be a good place for forwarding this message.


Date: Tue, 21 May 96 16:39:43 EDT  
From: List Manager 2
To: [log in to unmask]
Subject: Printed Circuit Board Lamination Process



Date: Mon, 20 May 1996 15:00:40 -0700 (PDT) 
From: Marc Siegel <[log in to unmask]>
Subject: Printed Circuit Board Lamination Process
     
A Printed Circuit Board company is looking for ways of eliminating, 
recycling  or at least reducing two wastes generated during the lamination 
process.  They are looking for a use for the edge trim which is generated 
during the process.  About 2 million pounds of edge trim are generated at 
their facilities worldwide each year.  The composition of the edge trim (in 
weight %) is:
     
Continuous Filament Fiber Glass          40-70% 
Epoxy Resin                              30-60%
DMF  (Dimethyl Formamide)                0.0015%  (1500 mg/g)
     
     
They are also looking for ways of eliminating, regenerating, or recycling 
the resin mixture left at the end of the process.  This resin solution 
contains a glycidyl ether of brominated bisphenol A, acetone, epoxy resin,
dimethyl formamide, phenyl glycidyl ether, amyl alcohol, and epichlorohydrin.
     
Thank you,
Marc

===================================================================
     
Dr. Marc H. Siegel
Project Coordinator, E-LYNX (US EPA ETI Program) 
Engineering Process & Information Consulting 
12397 Picrus Street
San Diego, CA 92129-4113
Phone:  619-484-9855
Fax:    619-484-9856
E-mail: [log in to unmask]
     
===================================================================

 Dean R. Cornstubble
 Research Chemical Engineer
 Research Triangle Institute (Pollution Prevention Program)
 Phone: 919-541-6813 (Fax, 7155)
 http://www.rti.org/units/ese/pp.html

------------------ RFC822 Header Follows ------------------
Received: by quickmail.llnl.gov with SMTP;22 May 1996 12:53:51 -0700
Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)
	 id OAA01961; Wed, 22 May 1996 14:50:06 -0700
Resent-Date: Wed, 22 May 1996 14:50:06 -0700
Received: by ipc.org (Smail3.1.28.1 #2)
	id m0uMHgg-0000O8C; Wed, 22 May 96 12:27 CDT
Resent-Sender: [log in to unmask]
Old-Return-Path: <[log in to unmask]>
Date: Wed, 22 May 1996 13:18:25 -0400 (EDT)
From: "Dean R. Cornstubble" <[log in to unmask]>
Subject: FAB: Fwd: Printed Circuit Board Lamination Process
In-reply-to: <[log in to unmask]>
To: [log in to unmask]
Message-id: <[log in to unmask]>
MIME-version: 1.0
Content-type: text/plain; charset=US-ASCII; X-MAPIextension=".TXT"
Content-transfer-encoding: 7bit
Priority: Normal
References: Conversation <[log in to unmask]> with
 last message <[log in to unmask]>
Resent-Message-ID: <"9E2IC2.0.s7H.Tvqen"@ipc>
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/4278
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]





ATOM RSS1 RSS2