Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0uLaSn-0000CCC; Mon, 20 May 96 14:17 CDT |
Old-Return-Path: |
|
Date: |
20 May 96 14:20:58 -0500 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
From [log in to unmask] Mon May 20 17: |
19:34 1996 |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"5HZ3M2.0.qeI.WLCen"@ipc> |
Subject: |
|
From: |
|
X-Status: |
|
X-Loop: |
|
Message-Id: |
<"Macintosh */PRMD=MOT/ADMD=MOT/C=US/"@MHS> |
Parts/Attachments: |
|
|
Is anyone aware of any reference book or review article available that
describes examples of PCB corrosion failures such as this green rust, along
with failure analysis to explain the chemical sources of the failures? My
reference books do not seem to cover this in any detail.
Edwin Bradley
Motorola
Ft. Lauderdale FL
________________________________________________________
To: [log in to unmask]@INTERNET
From: [log in to unmask]@INTERNET on Mon, May 20, 1996 12:48 PM
Subject: Re: FAB: Green rust
Resent-Date: Mon, 20 May 1996 11:05:43 -0700
Resent-Sender: [log in to unmask]
Old-Return-Path: <[log in to unmask]>
Resent-Message-Id: <"gXGJZ.0.ltA.LA9en"@ipc>
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/4221
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]
Doug,
The greenish material that you are seeing is most likely copper chloride.
It
means that you have a chloride-bearing material coming into contact with the
pins, corroding them.
Doug Pauls
CSL
[log in to unmask]
|
|
|