TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0uK3xI-0000EmC; Thu, 16 May 96 09:23 CDT
Encoding:
13 Text
Old-Return-Path:
Date:
Thu, 16 May 96 10:25:04 CST
From [log in to unmask] Thu May 16 13:
44:53 1996
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/4175
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"ExWCP.0.iN6.7fpcn"@ipc>
Subject:
From:
Precedence:
list
Resent-From:
Message-Id:
Parts/Attachments:
text/plain (16 lines)
          
          I'm almost embarrassed to ask this one.
          
          Green Cu oxide shows up on socket pins after about three 
          months in the field.  Very little shows up before assembly, 
          or shipment.
          
          Is this as simple as the wash not being monitored properly?
          
          I'll listen to anything as technical as anyone wants to get 
          from proper p.c. fab methods to the chemistry behind it.
          
          Thanks in advance.