TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
from simon.ipc.org by vnet.IBM.COM (IBM VM SMTP V2R3) with TCP; Thu, 09 May 96 12:23:37 EDT from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI) id LAA14569; Thu, 9 May 1996 11:08:20 -0700 by ipc.org (Smail3.1.28.1 #2) id m0uHWCO-0000PgC; Thu, 9 May 96 08:56 CDT
TO:
Old-Return-Path:
Date:
Thu, 09 May 96 09:52:47 EST
X-Loop:
Precedence:
list
Resent-From:
Cc:
Resent-Message-ID:
<"utX2P1.0.zfL.nbVan"@ipc>
Resent-Sender:
From:
Subject:
X-Mailing-List:
<[log in to unmask]> archive/latest/3979
Resent-Date:
Thu, 9 May 1996 11:08:20 -0700
Message-Id:
Parts/Attachments:
text/plain (85 lines)
     I realize that minimal gold (3-5 millionths) is best for soldering,
     but:
        a. Isn't that a pretty tight range?
        b. What if there is something on the other side, say, that will be
           used for wire bonding?


     MB


______________________________ Reply Separator
_________________________________
Subject: RE: BGA FInish
Author:  [log in to unmask] at SMTPLINK-HADCO
Date:    5/7/96 02:24 PM



Hi Gita,

Q:   What is the preferred surface finish for PWB's with PBGA packages?
A:   The critical process factors for BGA assembly are:
     * Surface Coplanarity
     * Solder Volume
     * Solderability
     * Moisture Sensitive (PBGA)
It 's okay to use Entek 106A, but you should consider the solderability of
second reflow or BGA  repair if there is any. Gold is very solderable, and
just as important, very coplanar.  It is increasingly becoming a popular
choice for SMD fine pitch board assemblies.  With gold, there is no
embrittlement concern as long as the thickness of  gold is 0.000003-5". You
can consider gold as an alternative to HASL.

Q:   Using Entek boards, what kind of flux is better to use, NO CLEAN or
 water soluble?
A:   No clean Flux is definitely a  better choice. According some technical
studies I read, water soluble is more likely to form solder balls if the
temperature profile and solder mask design are not optimum. In your case,
finding solder balls beneath the BGA is the last thing you want to see. With
no clean flux, the reduction in solid content will tightens the process
window and nitrogen atmosphere reflow  has proven helpful in improving
process yield when no clean flux is being used.

Thanks

[log in to unmask]


 ----------
From: TechNet-request
To: TechNet
Subject: FAB/ASSY: PREFERED PWB SURFACE FINISH FOR BGA
Date: Monday, May 06, 1996 2:08PM


     What is the preferred surface finish for PWB's with PBGA packages?

     I have been looking at some published industry data regarding PWA
     assemblies with plastic BGA's and so far all have had HASL surface
     finish and very little data on OSP (organic Solderability
     Preservatives such as Entek) coated boards.

     Has anyone had any OSP coated (Entek 106) mother board designs with
     BGA packages in production?
     What are the pro and con's with HASL Vs. ENTEK for BGA assembly?
     Using Entek boards, what kind of flux is better to use, NO CLEAN or
     water soluble?
     The preferred surface finish for assembling fine pitch components has
     become Entek (or Entek equivalent) for better coplanarity criteria,
     but is there a danger using Entek boards for BGA assembly?

     I would greatly appreciate any information you can share with me.