DESIGNERCOUNCIL Archives

1996

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vbKU7-0000UFC; Sat, 21 Dec 96 00:00 CST
Old-Return-Path:
Date:
Fri, 20 Dec 96 21:48:31 PST
Precedence:
list
X-Loop:
Resent-Sender:
DesignerCouncil-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/2269
TO:
Return-Path:
<DesignerCouncil-request>
From [log in to unmask] Mon Dec 23 12:
45:52 1996
Resent-Message-ID:
<"XICc91.0.p3M.1qtko"@ipc>
Subject:
From:
[log in to unmask] (James C. Patten)
Resent-From:
Message-Id:
Parts/Attachments:
text/plain (19 lines)
Jim,
 I am interested in the reservations about IPC-SM-782A for SMT land pattern
design. I have been designing to this latest spec and am fairly happy with the results. But I can always use a little help in this area. 

         Thanks
         James Patten

***************************************************************************
*   The mail list is provided as a service by IPC using SmartList v3.05   *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.*
***************************************************************************
* If you are having a problem with the DesignerCouncil, please contact    *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2