Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0ugJ68-0000MlC; Tue, 16 Jul 96 18:00 CDT |
Old-Return-Path: |
|
Date: |
Tue, 16 Jul 96 17:06:39 MST |
Precedence: |
list |
Resent-From: |
|
Cc: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
From [log in to unmask] Tue Jul 16 18: |
17:09 1996 |
Return-Path: |
<DesignerCouncil-request> |
Resent-Message-ID: |
<"fqcxc.0.Cq9.tx1xn"@ipc> |
Subject: |
|
From: |
|
TO: |
|
X-Loop: |
|
Resent-Sender: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Fred,
My experience with Scoring would lead me to suggest that
instead of scoring, place a short Route through the via
zone, just to improve the cut through the via.
Then, continue the rest of your score as usual
__________
------------(__________)--------
I have never experienced this with such thin laminate, but
expect that the barrels may be pulled out with such a small
hole wall for attachment.
Luck to ya,
Les Beller @ echostar
All,
Has anyone any experience using .010 FR4 for double sided boards? Also I
need to place 4- 0.025 dia plated thru holes centered on the edge of the
board. The board will be have to be panelized, so it will either be
V-Scored, punched, or routed (right through 1/2 of the dia of the holes. I
have been told that some companies are doing this, but I am sceptical. I
can't believe there will be any plating left. Has anyone done this, or do
you have any thoughts on the matter?
Regards
Fred Pescitelli
Phoenix Designs
1285 Turner Rd.
Lilburn, GA 30247
[log in to unmask]
770-923-3465
****************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05 *
****************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
****************************************************************************
****************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05 *
****************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
****************************************************************************
|
|
|