Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0uA0sf-00008pC; Thu, 18 Apr 96 16:04 CDT |
Encoding: |
69 Text |
Old-Return-Path: |
|
Date: |
Thu, 18 Apr 96 17:06:02 CST |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<DesignerCouncil-request> |
Resent-Message-ID: |
<"xYO1j1.0.uN9.hvgTn"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Sat Apr 27 16: |
02:44 1996 |
X-Loop: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
If you use the model of a piece of wire as being a resistor that heats
up when current passes through it (as it is and as it does), then
there should be no problem reading any graph that indicates rise above
ambient. This is where degree rise above ambient comes from.
Ralph, correct me if I'm wrong, but the assumption I've always heard
is that the air surrounding the wire is an infinite heat sink and its
temperature NEVER increases.
The other assumption is that temp rise above ambient can be roughly
linear. That means, if the chart says with a particular current you
get a 10 degree C rise above 20 degree C ambient, then you will get
basically (forgive me here) a 10 degree C rise at 40 degree C ambient
with the same current. Meaning your ABSOLUTE trace temperature is now
50 degree C.
When selecting hookup wire with insulation rated at a particular
temperature, these rise above ambient charts become critical.
Using the above info on traces (wire) covered with laminates
(insulation) becomes a little easier.
OK with you Ralph?
doug mckean
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Re[4]: heavy copper...
Author: [log in to unmask] at internet-mail
Date: 4/18/96 3:52 PM
Ben Davis wrote:
> ...So now I'm confused. Does the chart indicate the rise of the trace
> temperature or does it indicate the rise above ambient of the environment?
> Perhaps someone from the IPC committee that worked on the 275 (Gary are you
> there?) could comment and/or elaborate on the charts...
Note 3 of figure 3-4 says:
"For general use, the permissible temperature rise is defined as the
difference between the maximum safe operating temperature of the laminate
and the maximum ambient temperature in the location where the panel will
be used."
I agree that this and the other notes could have been written in a less
ambiguous way, however it seems evident to me that what you are seeing
as you look at the chart is that as the current rises the temperature
of the trace rises. The trace itself is the only thing defined in even
the most superficial of ways here. There is nothing said of the rest of
the environment (i.e.: thermal mass of surrounding parts, thermal
conductivity of the enclosure, air flow or heat transfer efficiency, etc...),
so, to
me, I don't see how any chart could ever hope to map the rise of the
ambient temperature due to current changes in a given conductor.
I would also welcome any comment from Gary or other authoritative source.
Or maybe just anyone with an opinion. :-)
____ [log in to unmask] "Nudists are people who wear
(.)(.) voice: (512)251-2341 one-button suits."
--000-(oo)-000--fax: (512)251-0498 --Anonymous
|
|
|