I noted Dave Hoover's response to the question about d.s. and he suggests
resin souyrce as the reason for variability between vendor "A" and "B". I
would suggest other possibilities such as treating tension, fabric tension
control at the weaver (also lot to lot!), etc. Unfortunately there are
probably also phantom variables.
Dave, a question. What is the magnitude of the "A" vs "B" vendor difference
in d.s. with for example FR-4? Anybody else have any data (or gut feel)
regarding the between-vendor variability for the "same" resin system?
Chet Guiles