JUST A LITTLE INFO THAT MIGHT BE OF HELP.
THROUGH THE PAST 2 YEARS I HAVE REQUIRED A .125" MOUNTING HOLE
WITH PADS CONNECTED GROUND FOR GROUNDING OUT A SCREW AND FRONT
PANEL. THE PAD I.D. IS .165" WITH A .075 WIDTH ON THE COMPONENT
SIDE USING A FULL CIRCULAR PAD. ON THE SOLDER SIDE TWO ARCS ARE
USED. FOLLOWING ARE ARC DEFINITIONS:
DRILL ORIGIN AT X,Y 0,0
ARC WIDTH .040
CENTERLINE OF ARC COORDINATES
X,Y FROM/TO -.080,.080 / .080,.080
X,Y FROM/TO -.080,-.080 / .080,-.080
NOTE: THE OPENINGS BETWEEN THE ARCS ON THE SOLDER SIDE MUST BE
PARALLEL TO THE WAVE TO INSURE THE HOLE WILL NOT FILL.
EXAMPLE: XXX
XX XX \
------------------------> WAVE
XX XX /
XXX