Subject: | |
From: | |
Date: | Tue, 21 Nov 95 13:55:25 EST |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Terpenes may work better for you than Axarel. Petroferm makes
terpenes for use in batch cleaners and benchtops. One warning is that
the fumes from the terpene can be very offensive to some people after
prolonged exposure.
______________________________ Reply Separator _________________________________
Subject: Cleaning of Roger's Duriod 6002/6010 Material
Author: [log in to unmask] at cc_gate
Date: 11/21/95 12:52 PM
We are currently using Duriod 6002/6010 type PWB's on one of
our products and are having problems cleaning the PWB's
after soldering and assembly operations. Removal of fluxes
and the cleaning fluid (Axarel) from this very hygroscopic
material has been difficult inspite of using the
Manufacturers recommended process. Any information
or sources of potential information relating to resolving
this situation would be appreciated.
[log in to unmask]
|
|
|