        I think it's more commonly coined a "bump" cycle. I've ran into 
     this when dealing with acrylic based adhesives such as flex circuitry. 
     When the press initially closes, this cycle would help eliminate any 
     air pockets trapped within the package. It's similar to "kiss" (or 
     double stage) lam cycles for thermoset resin systems. The initial low 
     pressure allowed the package to heat to melting temperatures before
     applying high pressure stage. This helps with high layer count PCBs
     that have very thin cores to manufacture them with. The thin cores
     can easily fracture and generally have very fine lines that can be 
     stressed when high pressure is directly applied. (Vacuum assist
     lamination has virtually replaced all these various techniques)
     
     Hadco Printed Circuits
     Tech Center Two / Watsonville                
     
     
     _/_/_/_/_/_/_/  _/_/_/_/   _/_/_/_/_/_/  _/_/_/_/_/_/
         _/_/      _/              _/_/         _/_/
       _/_/      _/              _/_/         _/_/
     _/_/       _/_/_/_/   _/_/_/_/_/_/ _/_/_/_/_/_/
     
     
     Dave Hoover              (408) 728-6677 
     Senior Process Engineer  (408) 728-1728 Fax 
     [log in to unmask]
     
     


______________________________ Reply Separator _________________________________
Subject: Burp Cycle!
Author:  [log in to unmask] at SMTPLINK-HADCO
Date:    10/16/95 4:15 PM


I recently heard reference to a lamination press cycle for multilayer PCB's 
as a burp cycle.  This cycle is intended to help with air entrapment I believe.
     
If anybody has any specifics on this cycle and or results of if it works or 
not I would appreciate any and all feedback.
     