Does anyone have any experience at backboard heating for PTH
soldering? The laminate material is polyimide and is .090" thick.
Typical components include radial and axial leaded devices as well as
DIP packages.
We are trying to find ways to assist in high temp soldering (MP of
300degC or Eutectic @ 280degC).
What we are looking for are vendor recommendations and/or any
technical comments that may be available.
Please fell free to contact me @ (713) 987-4365 or return Email to
DRAKE@SSDSRDCC
Thanks in advance,
Darrell Drake