Is there any statistical data on the long term reliability of tabs plated 
at less than the standard of 30 microinches? There have been requests for 
30 micro" average from some shops, but no reliability data to back up the 
requests. I have even seen SIMMs with flash gold surface-not for us, but 
used to try to sell us on flash gold tabs for type I boards. Is this used 
anywhere for SIMMs?

What are the concerns with thinner gold? ..Ni migration and oxidation? 
I have heard there are some guys building Ni coated tabs without gold. Is 
this elemental Ni?