Subject: | |
From: | |
Date: | Fri, 05 May 95 14:53:59 PST |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Kelly,
From Enthones data sheet, the dielectric strength is listed as
>500 VDC. This should be volts per mil. If you need additional
information, you can contact our Enthone technical rep (Greg Beck)
at 800-548-9801, ext/box 7213
Hope this helps.
John
______________________________ Reply Separator _________________________________
Subject: Enthone DSR 3241 Solder Mask
Author: [log in to unmask] at corp
Date: 5/4/95 4:06 PM
From: Kelly Kovalovsky, Raw Card Quality Engineering
_ Phone:704-595-7336 Tie Line:795-7336 FAX Ext. 4727
Subject: Enthone DSR 3241 Solder Mask
Can someone provide me with the dielectric strength of Enthone DSR
3241 solder mask?
Kelly Kovalovsky
IBM Microelectronics Division
6800 IBM Drive MG12/251
Charlotte, NC 28262-8563
|
|
|