Subject: | |
From: | |
Date: | Wed, 26 Apr 95 10:22:00 EST |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
The EMPF HelpLine has received a request to locate a source of specialty
circuit boards. Ultimate use of the assembly will be as a environmental
sensor. The base board material (epoxy glass has been used in the past) is
"coated" with a contiguous aluminum through whatever process, nominal
thickness approx. .027" or thicker if possible. The aluminum is then
patterned through some subtractive process (chemical or mechanical). Other
processes will ultimately be accomplished to the board, but initial need is
to find someone who can do this part of the process. End item is proprietary
and patent pending at present and non-disclosure documents will be required.
Respond either through this TechNet, or e-mail to
[log in to unmask], phone 317.26.5616 fax 317.26.5615.
|
|
|