Mr. Li,
Could you be more specific in your question? I have been closely involved in
all of the phases of the Cleaning and Cleanliness Test Program. What aspect
of control are you interested in: flux amount, handling, etc? I wrote the
majority of the text for TR-582, so if you could contact me, I could explain
further.
Douglas Pauls
Contamination Studies Laboratories
[log in to unmask]