Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0tMuZe-0000M1C; Tue, 5 Dec 95 04:26 CST |
Old-Return-Path: |
<miso!fgf1s1.merix.com!Paul=Formiller%Eng%ECB> |
Date: |
Mon, 4 Dec 95 14:56:29 PST |
Precedence: |
list |
X-Loop: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
From [log in to unmask] Sat Apr 27 15: |
25:03 1996 |
TO: |
|
Return-Path: |
|
Resent-Message-ID: |
<"rexdV.0.GEA.0v1nm"@ipc> |
Subject: |
|
From: |
|
Resent-From: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
In my experience the current IPC test used by laminators to check dimensional
stability has no correlation to dimensional stability results after multilayer
lamination at a PCB shop. Is IPC investigating a different test method or
does any PCB shop have there own "dimensional check" for incoming laminate.
I'm working on this issue at our facility and I'd like to swap ideas with
other PCB shops.
Thanks in advance for any response.
Paul Formiller
Process Engineer - Merix Loveland
[log in to unmask]