contact your nearest Alpha Metals sales office or call the office in
Jersey City NJ 201.434.6778 and ask for Dr. Ken Gilleo
______________________________ Reply Separator _________________________________
Subject: Conductive Epoxy
Author: [log in to unmask] at corp
Date: 12/20/95 2:18 PM
We have an urgent need for one (1) or two (2) each 30 ml syringe of
electrically conductive epoxy. We need an epoxy that, when cured, will
withstand temperture cycling in outdoor applications anywhere in the world.
That could be a desert environment with cold nights and hot days, to just plain
hot jungle, to North Slope area. Something that can handle say, -50 deg C to
+65 Deg C or better. We would be using and EFD type pneumatic dispenser to
apply it.
Everything we know of is on the East coast and is snowed in right now, so they
cannot ship tonight. Does anyone have a lead on an immediate West coast source?
We really need it tomorrow.
MANY thanks in advance,
Charles Barker
Input/Output, Inc.
713/276-3328
|
|
|