Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0tRsS4-0000NSC; Mon, 18 Dec 95 21:10 CST |
X-PS-Qualifiers: |
/FONT=Courier-Bold/LINES=66/LEFT_MARGIN=36/CALCULATE/TOP_MARGIN=36/BOTTOM_MARGIN=36 |
X-VMS-Cc: |
DOUG_M2 |
Date: |
Mon, 18 Dec 1995 16:32:59 -1000 |
MIME-version: |
1.0 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
From [log in to unmask] Sat Apr 27 15: |
31:27 1996 |
TO: |
|
Return-Path: |
|
X-Loop: |
|
Old-Return-Path: |
<miso!sfov1.verifone.com!DOUG_M2> |
Resent-Message-ID: |
<"xDwuP.0.WZF.xqYrm"@ipc> |
Subject: |
|
Message-id: |
|
X-VMS-To: |
|
Content-transfer-encoding: |
7BIT |
Organization: |
VeriFone |
From: |
|
Parts/Attachments: |
|
|
Yes, what Tom is saying is completely correct! The problem occurs when
your design places the ceramic capacitors to close to the edge or to colse
to the V-cut used a the break away. If you make a special fixture you
still need to avoid clamping down directly on the SMT component parts and
so you still have to bendo or flex the board during the separtation of the
various pannelized boards or when breaking away the breackaways after SMT
and PTH assembly is complete. So you must set your design rules to place
these capacitors further inboard from the edges than you would like.
Once you have done this the problem will go away, at least where my boards
are concerned!
Best
Doug Mills
From: IN%"[log in to unmask]" 18-DEC-1995 09:57:55.14
To: IN%"[log in to unmask]"
CC:
Subj: Cracking Capacitors
Another source for information regarding cracked capacitors is through the
Surface Mount Technology Association Academy. I attended a very excellent
seminar given by John Maxwell entitled: "Surface Mount Problem Solving:
Design and Production" where a great deal of time was spent on ceramic chip
cracking.
Two items mentioned which may get you started are (A) most failures of this
type occur at the de-paneling stage and (B) the positioning of the crack on
the chip may point to the failure mechanism.
I surely hope that at least the s.m.t.a. reference source may assist you.
Happy Holidays!
Tom Eshelman, Enthone-OMI
1.800.548.9801 ext. 7257
[log in to unmask]
Return-path: <[log in to unmask]>
Received: from HNLVX by sfov1.verifone.com (PMDF V4.3-7 #5451)
id <[log in to unmask]>; Mon, 18 Dec 1995 09:57:42 -1000
Received: from TPEV1 by verifone.com (PMDF V4.3-7 #5449)
id <[log in to unmask]>; Mon, 18 Dec 1995 07:58:10 -1000
Received: from HNLVX by tpev1.verifone.com (PMDF V4.3-7 #5453)
id <[log in to unmask]>; Tue, 19 Dec 1995 01:53:40 +0800
Received: from SFOV1 by verifone.com (PMDF V4.3-7 #5449)
id <[log in to unmask]>; Mon, 18 Dec 1995 07:53:28 -1000
Received: from simon.ipc.org (168.113.24.64)
by sfov1.verifone.com (PMDF V4.3-7 #5451)
id <[log in to unmask]>; Mon, 18 Dec 1995 09:52:29 -1000
Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)
id JAA10047; Mon, 18 Dec 1995 09:34:34 -0800
Received: by ipc.org (Smail3.1.28.1 #2) id m0tRjT5-0000MIC; Mon,
18 Dec 95 11:35 CST
Resent-date: Mon, 18 Dec 1995 09:34:34 -0800
Date: Mon, 18 Dec 1995 11:39:38 -0500
Resent-from: [log in to unmask]
From: [log in to unmask]
Subject: Cracking Capacitors
Resent-sender: [log in to unmask]
To: [log in to unmask]
Resent-message-id: <"2Tew-3.0.JmE.CPQrm"@ipc>
Message-id: <[log in to unmask]>
Content-transfer-encoding: 7BIT
Old-Return-Path: <miso!aol.com!TMEshelman>
X-Mailing-List: <[log in to unmask]> archive/latest/2086
X-Loop: [log in to unmask]
Precedence: list
|
|
|