Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0tNiQm-0000MaC; Thu, 7 Dec 95 09:40 CST |
Old-Return-Path: |
<miso!psion.com!Mike-Fugl> |
Date: |
Thu, 07 Dec 95 08:26:34 GMT |
Precedence: |
list |
X-Loop: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
From [log in to unmask] Sat Apr 27 15: |
26:17 1996 |
TO: |
|
Return-Path: |
|
Resent-Message-ID: |
<"ED6hg3.0.wGL.Uhmnm"@ipc> |
Subject: |
|
From: |
|
Resent-From: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
I would be interested in assisting you in your investigation. However
I think to be useful you must define ppm more closely.
Ideally the metric must:
1)take into account the complexity/density of interconects per unit
area.
2) Define the causes of failure to be included. EG: Misplaced
components should not be counted as having dry's or shorts, but
measured separately.
3) Be realistic. You cannot count the exact number of opens/shorts
from failed PCBs at ICT, merely the event and it's cause. A component
with a quantity of shorts or drys on a single IC will inevitably be
recorded as simply Dry IC? or Short IC?
I will be happy to provide you with our ICT results.
Regards
Mike Fugl
Snr Prod Eng
Psion.
______________________________ Reply Separator _________________________________
Subject: PWB Solder defect rates
Author: [log in to unmask] at INTERNET
Date: 7/12/95 8:38 AM
I am interested in actual soldering defect rates found "out there".
While visiting a main customer, I was shocked to hear that the number of
open circuits detected at "in-circuit testing" was running around 25 ppm.
Apparently this problem is due to insufficient solder during surface mount
assembly and is due to many different causes. This value of 25 ppm was
stated as "above average" but at the same time was considered "okay" due to
the complexity and large number of interconnects on the pcb's. I would like
to ask the following questions:
1) Can anyone share their actual "solder open" defects rates and
provide how they compare with the industry average? (I would
attempt to establish the distribution curve of responses and
publish later) Can you include bare board finish (ie HASL, reflow
tin-lead, OSP etc...)?
2) Is this considered normal???
3) Is there a repair procedure recommended by IPC to repair these types
of defects and is there a reference IPC document?
4) How are the defect rates normalized based upon assembly complexity,
board size and SMD pad geometries?
5) Has this defect rate been "self-inflicted" with the advent of
no-clean fluxes and solder paste?
Thanks
Dave Rooke - Circo Craft